Check detectors to compare

Compare detectors
Check to
compare
Name Material Type Immersion Cooling Wavelength Package Window Detectivity Time constant
PCI-4TE-12 MCT Photoconductive Immersion
Four-stage
12 TO8
TO66
wedged ZnSe AR coated
\(≥2,0x10^{9}\) \(≤7\)
PVI-2TE-10,6 MCT Photovoltaic Immersion
Two-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥1,0x10^{10}\) \(≤10\)
PVI-3TE-10,6 MCT Photovoltaic Immersion
Three-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥1,5x10^{9}\) \(≤10\)
PVMI-2TE-8 MCT Multiple junction Immersion
Two-stage
8 TO8
TO66
wedged ZnSe AR coated
\(≥2,0x10^{9}\) \(≤4\)
PVMI-3TE-8 MCT Multiple junction Immersion
Three-stage
8 TO8
TO66
wedged ZnSe AR coated
\(≥3,0x10^{9}\) \(≤4\)
PVMI-3TE-10,6 MCT Multiple junction Immersion
Three-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥1,5x10^{9}\) \(≤3\)
PVMI-4TE-8 MCT Multiple junction Immersion
Four-stage
8 TO8
TO66
wedged ZnSe AR coated
\(≥6,0x10^{9}\) \(≤4\)
PVMI-4TE-10,6 MCT Multiple junction Immersion
Four-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥2,0x10^{9}\) \(≤3\)