Name Material Type Immersion Cooling Wavelength Package Window Detectivity Time constant
PCI-2TE-9 MCT Photoconductive Immersion
Two-stage
9 TO8
TO66
wedged ZnSe AR coated
\(≥4,0x10^{9}\) \(≤40\)
PCI-2TE-10,6 MCT Photoconductive Immersion
Two-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥1,0x10^{9}\) \(≤10\)
PCI-2TE-12 MCT Photoconductive Immersion
Two-stage
12 TO8
TO66
wedged ZnSe AR coated
\(≥4,5x10^{8}\) \(≤3\)
PCI-2TE-13 MCT Photoconductive Immersion
Two-stage
13 TO8
TO66
wedged ZnSe AR coated
\(≥2,3x10^{8}\) \(≤2\)
PVI-2TE-8 MCT Photovoltaic Immersion
Two-stage
8 TO8
TO66
wedged ZnSe AR coated
\(≥2,0x10^{9}\) \(≤45\)
PVI-2TE-10,6 MCT Photovoltaic Immersion
Two-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥1,0x10^{10}\) \(≤10\)
PVMI-2TE-8 MCT Multiple junction Immersion
Two-stage
8 TO8
TO66
wedged ZnSe AR coated
\(≥2,0x10^{9}\) \(≤4\)
PVMI-2TE-10,6 MCT Multiple junction Immersion
Two-stage
10,6 TO8
TO66
wedged ZnSe AR coated
\(≥1,0x10^{9}\) \(≤3\)